Inicio / Conocimiento / Pinholes and blisters
Pinholes and blisters

Notas de ingeniería. No un blog. Pinholes and blisters are not the same failure. Pinholes are outgassing y porosity. Blisters are moisture or vapour bajo a fresh film. Therefore the repair is not the same coat.
Pinholes and blisters after a cold membrana
Prime, wait, then apply at the build in the current TDS. Porosity Sealer and Imprimación Epoxi Plus are the catalogue names for prepared concrete before a cold membrana. Humidity Imprimación is the name when residual moisture is the issue. Imprimación Epoxi 100 is listed separately.
Repair is cut-back. It is not another thin roll over the bubble. The next coat still follows the overcoat interval on the sheet for that membrana and finish. Colodur Eco (aliphatic finish) has its own window.
However, site-failure language on this site is a specifier note. It is not a substitute for the method statement issued with the current TDS. In addition, do not invent kg/m².
What to write in the specification
First, name the imprimación. Then name the membrana. After that, name the finish. Read consumo from the current TDS, then the calculadora.
See Porosity Sealer, Imprimación Epoxi Plus, and documents.
Outbound reference: EOTA.
A blister that is rolled over will return. Cut back, then recoat inside the window on the sheet.
Therefore the current TDS remains the source for mix ratio, overcoat and consumo. Then the calculadora sizes the area. However, a number invented here would be a specification error. In addition, the application page is the schedule. First name the exposición. Next name the commercial product and the chemical type in the same sentence. After that, open documents. Also keep the finish on the same clause as the body. A sample, a colour or a photograph does not replace that sentence.
These notes do not replace the current TDS, SDS or a written specification. For pack sizes, mix ratio and kg/m², read the ficha vigente, then the calculadora.